For this purpose, the commercial software ESI SYSWELD was adopted, since it is one of the most advanced tools for this purpose. In this communication, T-joint welded configurations are investigated, considering arc welding and laser beam welding processes. Considering these changes and the materials properties at the different temperature values, it is possible to obtain reliable models of the welding processes.

The most advanced tools take into account the thermo-metallurgical and thermo-mechanical changes that take place during the welding processes. Abstract Advances in computational tools for welding process simulation have been noteworthy, allowing to assess complex phenomena, as is the case of welding distortion and residual stress.